Starting on my first attempt forming Kydex interior panels. My thinking is I would abuse whatever is on the walls and at least I could replace the kydex down the road. Also can access and inspect my work behind the panels easier and more frequently. My plan is to use .028" material (0.197 lbs/sq ft) as much as possible for weight considerations.
Just looking for suggestions from those that have experience with beading and forming flanges with the .028" kydex material? Tape on the the bead rollers to minimize defects? When is cold forming ok vs adding a little heat?
Mark Moyle - I never could get to that Facebook video link you posted previously. Not sure if that operator error on my part?
Any and all help and suggestions appreciated.
Just looking for suggestions from those that have experience with beading and forming flanges with the .028" kydex material? Tape on the the bead rollers to minimize defects? When is cold forming ok vs adding a little heat?
Mark Moyle - I never could get to that Facebook video link you posted previously. Not sure if that operator error on my part?
Any and all help and suggestions appreciated.
Comment